Movie S4.

Electrodeposition of lithium in the electrolyte 1M EC/DMC LiPF6 using crosslinked nanoparticles having r.c.p. pore size of 100 nm at a current density of 8 mA/cm2 for 1500 seconds, shortened to 10 seconds.

Confining electrodeposition of metals in structured electrolytes

Snehashis Choudhury, Duylinh Vu, Alexander Warren, Mukul D. Tikekar, Zhengyuan Tu, and Lynden A. Archer