For a peeling sample of the middle layer of A:B = 15:1, the sample peels through the middle layer, the peeling toughness is almost the same as the bulk toughness (over 300 J/m2), and the middle layer leaves residuals on both peeled arms.

Stretchable materials of high toughness and low hysteresis

Zhengjin Wang, Chunping Xiang, Xi Yao, Paul Le Floch, Julien Mendez, and Zhigang Suo