Movie S1.

Activation of NP-control in 1.5 mm-thick PDMS. No visible color change demonstrates that the applied 3.2 MPa does not provide sufficient thermal energy to cause NP isomerization. Scale bar = 2.5 mm.

High-intensity focused ultrasound-induced mechanochemical transduction in synthetic elastomers

Gun Kim, Vivian M. Lau, Abigail J. Halmes, Michael L. Oelze, Jeffrey S. Moore, and King C. Li

PNAS. 2019. 116:10214-10222 DOI: 10.1073/pnas.1901047116