Movie S2.
Large-area view of the same process in Supplementary Movie S1, showing the uniform growth of super-cooled sulfur everywhere on the Ni pattern. Play speed is 32x of the actual speed.
Large-area view of the same process in Supplementary Movie S1, showing the uniform growth of super-cooled sulfur everywhere on the Ni pattern. Play speed is 32x of the actual speed.